Solid polymer : Dissolve by supplying solid polymer and water in a certain proportion.
Liquid polymer : Supply the liquid polymer stock solution and water in a certain proportion and dilute the stock solution.
Solid + liquid : Mix solid + liquid polymer and water in a certain proportion.
Solid polymer and liquid polymer can be used individually or simultaneously.
Can be converted to liquid in winter or when solubility of the solid polymer cannot be secured.
Prevention of coagulation and residual phenomenon of solid polymer by forming a water film around the partial vortex into which the solid polymer is injected
By installing a heating device in the dissolution tank, the melting temperature is maintained and the polymer lump phenomenon is prevented.
Model name | Capacity (m3/hr) Solid/liquid |
Drive (kW) |
Weight(Ton) Static (dynamic) load | Solubility |
Tank | Size (mm) | ||
---|---|---|---|---|---|---|
W | L | H | ||||
K-HYPAD500 | 0.5/0.75 | 1.2 | 0.35(0.8) | 900 | 1440 | 600 |
K-HYPAD1000 | 1/1.5 | 1.5 | 0.45(1.5) | 900 | 1860 | 750 |
K-HYPAD2000 | 1.5/2 | 2.65 | 0.6(2.6) | 1000 | 2000 | 1000 |
K-HYPAD3000 | 2/3 | 2.65 | 0.8(3.8) | 1100 | 2320 | 1200 |
K-HYPAD4000 | 3/4 | 2.65 | 1.0(5.0) | 1350 | 2440 | 1230 |
K-HYPAD5000 | 3.5/5 | 5 | 1.3(6.3) | 1420 | 2950 | 1230 |
K-HYPAD6000 | 4/6 | 5 | 1.6(7.6) | 1400 | 2950 | 1534 |
K-HYPAD8000 | 6/8 | 5 | 2.0(10.0) | 1400 | 3800 | 1534 |
K-HYPAD10000 | 7.5/10 | 7 | 2.5(12.5) | 1600 | 4200 | 1534 |
K-HYPAD15000 | 10/15 | 11.5 | 3.5(18.5) | 2000 | 5100 | 1534 |